?A quick and effective method of cleaning objects prior to plating. The cleaning process uses an electrolytic bath, similar to plating operations. The 2 lb. size makes 8 gallons – 5 lb. size makes 20 gallons. Use with a stainless steel anode. Clean with the solution heated from 120¬_ to 160¬_ F (50¬_ to 71¬_ C) at 2 to 6 volts for 15 to 30 seconds.